Knowledge Base › Structural Design Error Case Study › Uneven Annealing Heating Causing Plate Side Bow

Uneven Annealing Heating Causing Plate Side Bow

E42-230 · Heat Treatment Distortion and Cracking · 65Mn Spring Steel Plate · ★★★

Problem Description

After annealing, the steel plate side-bows 3mm over full length; difficult to level.

Root Cause

[Uneven Heating] Furnace temperature difference 60℃; phase transformation out of sync across the plate. [Side Bow] Uneven residual stress after cooling gives 3mm side bow. [Design Omission] Non-uniform loading, no hot-air circulation.

Corrective Solution

1. Add forced hot-air circulation in the furnace.
2. Keep loading spacing ≥50mm for uniform temperature.
3. Control heating rate to ≤80℃/h.
4. Slow cool with the furnace.
5. Level with a roller leveler after discharge.
6. Measure side bow each batch.
7. 100% hardness-uniformity check.
8. Annual calibration of furnace temperature uniformity.

Checklist

Reference

GB/T 3279-2009

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »