E42-238 · Stress Concentration · Large Gear Spoke · ★★★
After 1.5 years of operation, web-hole edges crack and propagate to the rim.
[Hole-Edge Stress] Lightening holes not chamfered; K_t=3; spoke bending σ=90MPa. [Fatigue Crack] Alternating centrifugal + bending cracks hole edges after 1.5 years. [Design Omission] Sharp hole edges, not strengthened.
1. Chamfer lightening holes on both sides R3.
2. Shot-peen strengthen hole edges.
3. Thicken spokes to 1.2t.
4. Balance the gear.
5. Open cover and magnetic-particle inspect annually.
6. Weld repair per qualification.
7. Speed-limit operation to lower stress.
8. Fatigue check each batch.
GB/T 10095.1-2008