E42-419 · Stress Concentration · HSG-100 Cylinder Bottom · ★★★
HSG-100 cylinder bottom (Φ160) transition fillet r=2mm cracks and leaks; 2 replaced per month
[Small Transition] Bottom transition r=2mm (should be ≥8mm); Kt=2.7. [Crack] Internal pressure σ=240MPa; fillet cracks. [Design Omission] Not ground after forging; wall not measured; safety factor 1.2 (should be ≥2.0).
1) Transition r≥8mm;
2) Forging flow lines follow bottom shape;
3) Magnetic-particle fillet;
4) Re-measure wall thickness;
5) Limit pressure;
6) Add leak monitor;
7)NDE;
8) Replace at end of life.
GB/T 13342-2007