Shaft-Shoulder Runout Groove Sharp-Corner Stress Concentration

E42-469 · Stress Concentration · Drive Shaft · ★★★

Problem Description

Drive shaft (φ60) shoulder runout groove sharp corner fractures; shaft breaks; 1 rejected per month

Root Cause

[Sharp Corner] Runout groove R=0.2mm; Kt=3.5; σ=320MPa.
[Fracture] Stress-concentration crack.
[Design Omission] No larger fillet; load not limited; safety factor 1.2 (should be ≥2.5).

Corrective Solution

1) Runout groove R≥2mm;
2) Enlarge shaft diameter to 75mm;
3) Shot-peen strengthen;
4) Smooth transition;
5) NDE each batch;
6) Limit working load;
7) Upgrade material to 42CrMo;
8) Periodic re-measurement.

Checklist

Reference

GB/T 3077-2015