E42-522 · Stress Concentration · Drive Shaft (45 Steel) · ★★★

Problem Description

Shoulder r=1mm; Kt=2.5; cyclic fracture; 3 shafts broken per year

Root Cause

[Stress Concentration] r=1mm; Kt=2.5; local σ=Kt·σn exceeds yield.
[Fatigue] Alternating load.
[Design Omission] R too small; no transition; safety factor 1.1 (should be ≥1.5).

Corrective Solution

1) Raise R to 6mm;
2) Add relief groove;
3) Surface quench;
4) Crack-check each shaft;
5) Limit load;
6) Polish;
7)NDE;
8) Periodic re-measurement.

Checklist

Reference

GB/T 3075-2008

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL