E42-523 · Stress Concentration · Reactor (φ1600) · ★★★
Nozzle opening unreinforced; stress concentration factor 2.8; weld cracks; repaired 2 times per year
[Opening Concentration] Unreinforced; local σ=2.8σm exceeds allowable.
[Welding] Heat-affected zone brittle.
[Design Omission] No reinforcing ring; no analysis; safety factor 1.2 (should be ≥2.0).
1) Add reinforcing ring;
2) Integral reinforcement;
3) Grind smooth;
4) Crack-check each furnace;
5) Limit pressure;
6) Post-weld heat treatment;
7)NDE;
8) Periodic re-measurement.
GB/T 150.3-2011