E42-076 · Thermal Distortion & Thermal Stress · Ground Workpiece 40Cr · ★★
Grinding heat causes a dimensional drift of 0.01mm (allowable 0.005)
[Grinding Heat] With a specific grinding energy q'=60J/mm³ the workpiece temperature rises 30℃, and with aluminium α=23e-6 and a length of 200mm the elongation Δ=αLΔT=23e-6×200×30 is of the order of 0.138mm.
[Dimensional Drift] Insufficient cooling makes the dimension change in real time and exceed tolerance.
[Design Omission] Cooling was not sufficient and the measurement was not taken at a uniform temperature, so the drift exceeded tolerance by 2 times.
1) Provide high-pressure coolant at the grinding zone with a flow of ≥40L/min;
2) Stop the wheel at intervals and measure at a uniform temperature;
3) Select a wheel with a low heat generation grade;
4) Use more passes with smaller depth of cut to reduce heat;
5) Pre-cool the workpiece to room temperature before measuring;
6) Measure the dimension online and compensate;
7) Control the coolant concentration at 5%;
8) Include thermal drift in the process.
JB/T 9901-2012 Cylindrical Grinders — Inspection of Accuracy