E42-125 · Thermal Distortion & Thermal Stress · Motor Rotor with Hot-Fit Bearing · ★★
After the hot fit the bearing internal clearance is negative and the bearing seizes during warm-up
[Interference Contraction] The bearing heated to 80℃ is pressed onto the shaft, and after cooling the interference combines with the axial contraction so the internal clearance becomes negative.
[Seizure] A negative clearance plus thermal expansion during running locks the bearing.
[Design Omission] No cold clearance margin was left and the heating temperature was too high.
1) Measure the cold clearance before the hot fit and leave a margin;
2) Control the heating temperature at 80~100℃;
3) Heat uniformly by induction;
4) Measure the clearance after assembly and confirm it is at least the design value;
5) Monitor the running temperature rise;
6) Precision grind the journal;
7) Re-measure the clearance after cooling;
8) Include the hot-fit clearance in the process.
GB/T 307.1 Rolling Bearings — Tolerances