E42-527 · Thermal Deformation and Thermal Stress · Cast Iron Platform (2000×1500) · ★★
Platform locally heated and warped 0.15mm, exceeding the 0.05 allowance, poor flatness; 2 pieces returned per month
[Thermal Warping] Local ΔT=150, thermal stress exceeding yield warped 0.15mm.
[Restraint] Rigid fixing.
[Design Omission] No uniform heating and no stress release; safety factor 1.3 (should be ≥2.0).
1) Uniform heating;
2) Add ribs for higher stiffness;
3) Aging treatment;
4) Flatness check each piece;
5) Limit temperature difference;
6) Slow cooling;
7)Stress relief;
8) Periodic re-measurement.
GB/T 22095-2008