Non-Uniform Hardness After Quenching Causes the Guide Rail to Be Ploughed

E42-038 · Linear Guide Accuracy · Linear Guide Rail · ★★★

Problem Symptom

Scratches and scoring occur where the local hardness is low

Root Cause

[Hardness Variation] Non-uniform quenching gives HRC52-60 with soft zones.
[Ploughing] The soft HRC52 zones are ploughed by hard particles, producing scratches 0.1mm deep.
[Design Omission] The hardness band was not controlled and no flaw detection was performed, so scoring occurred.

Correct Solution

1) Quench the rail as a whole for a uniform structure;
2) Control the hardness band to HRC58-62;
3) Perform magnetic-particle inspection and hardness checks;
4) Superfinish grind to Ra0.4;
5) Keep assembly clean and chip-free;
6) Provide forced lubrication;
7) Carry out an accuracy inspection before shipment;
8) Include the hardness band in incoming inspection of guide rails.

Checklist

References

GB/T 1299 Tool Steels

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL