Straightness Out of Tolerance After Scraping Causes a Step in the Machined Surface

E42-088 · Linear Guide Accuracy · Machine Tool Cast Iron Guide Rail · ★★

Problem Symptom

Straightness 0.03 over the full length, steps appear on the machined surface

Root Cause

[Straightness] The straightness after scraping is out of tolerance at 0.03mm over the full length (0.01mm required).
[Step] The undulation of the moving parts produces a step on the machined surface.
[Design Omission] The contact spots were not checked and the straightness was not measured by laser, so steps appeared.

Correct Solution

1) Scrape the guide to 25 points per 25×25mm;
2) Measure the straightness with a laser interferometer;
3) Keep the scrape pattern consistent;
4) Finish the datum face first;
5) Re-inspect under load;
6) Re-scrape parts that show steps;
7) Maintain the accuracy periodically;
8) Make the straightness a mandatory inspection item.

Checklist

References

GB/T 17421.1-1998 Machine Tools — Geometric Accuracy

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »