E42-327 · Residual Stress Deformation · Quenched thin-plate part · ★★
Thin plate (δ=4): warpage 0.5mm after quench, grinding allowance insufficient; 4 pieces scrapped monthly
[Quench distortion] Uneven cooling, martensite transformation variation caused warpage.
[Residual stress] σ=200MPa.
[Design Omission] No die quenching, no cooling control; safety factor only 1.3.
1) Die-quench mold to limit distortion;
2) Martempering for cooling;
3) Uniform spray cooling;
4) Temper stress relief;
5) Flatness check each batch;
6) Leave 0.3mm grinding allowance;
7) Limit quench temperature;
8) Mechanical straightening.
GB/T 16923-2008