E42-494 · Residual Stress Deformation · Quenched part · ★★

Problem Description

Quenched part (40Cr) grinding stress crack 15mm long, scrapped; 3 pieces scrapped monthly

Root Cause

[Grinding stress] Grinding heat caused surface tensile stress σ=400MPa and crack.
[Crack] Surface network cracking.
[Design Omission] No feed control, no cold quench; safety factor 1.3 (should be ≥2.0).

Corrective Solution

1) Control grinding feed 0.01mm;
2) Ample cooling;
3) Lower grinding wheel hardness;
4) Temper after rough grinding;
5) NDE each piece;
6) Limit grinding speed;
7) Switch to CBN wheel;
8) Periodic re-measurement.

Checklist

Reference

GB/T 1184-1996

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL