Excessive Screw-to-Barrel Clearance in an Injection Moulding Machine Poorly Plastifies

E43-118 · Improper Clearance Fit · Injection Moulding Machine · ★★

Problem Symptom

The clearance between the Φ45 screw and the barrel was designed at 0.20mm but measured 0.65mm; plasticising output fell 12%

Root Cause

[Large Clearance] The design clearance was 0.20mm, but barrel wear opened it to 0.65mm and it was never replaced.
[Backflow] With the large clearance the melt flowed back, cutting plasticising output by 12% and causing short shots.
[Design Omission] The clearance should have been controlled to ≤0.25mm with the barrel hard faced, but no wear replacement interval was defined.

Correct Solution

1) Control the clearance to ≤0.25mm;
2) Hard face the barrel bore;
3) Measure the clearance every 6000h;
4) Nitride the screw;
5) Carry out a plasticising output test;
6) Verify against the backflow;
7) Provide a check ring;
8) Replace as soon as the limit is exceeded.

Checklist

References

GB/T 1801-2009 Limits and Fits