Excessive Screw-to-Barrel Clearance in a Twin-Screw Extruder Degrades the Material

E43-119 · Improper Clearance Fit · Twin-Screw Extruder · ★★

Problem Symptom

The clearance between the screw and the barrel was designed at 0.15mm but measured 0.55mm; shear heating raised the melt temperature and the material degraded

Root Cause

[Large Clearance] The design clearance was 0.15mm, but barrel wear opened it to 0.55mm.
[Degradation] With the large clearance the material stagnated in the dead zone and was sheared and overheated, so it degraded and discoloured.
[Design Omission] The clearance should have been controlled to ≤0.20mm with the temperature controlled, but no wear replacement interval was defined.

Correct Solution

1) Control the clearance to ≤0.20mm;
2) Use a replaceable barrel liner;
3) Control the temperature difference ΔT≤10℃;
4) Measure the clearance every 5000h;
5) Measure the melt temperature;
6) Verify the temperature rise against the stagnation;
7) Provide a venting section;
8) Replace as soon as the limit is exceeded.

Checklist

References

GB/T 1801-2009 Limits and Fits