Insufficient Rotor-to-Shaft Interference Causes Slipping

E43-055 · Interference Fit Failures · Inverter Motor Rotor · ★★★

Problem Symptom

Designed interference between rotor and shaft was 0.03mm but measured 0.015mm; high-speed slipping caused a 40℃ temperature rise and destroyed 2 units

Root Cause

[Insufficient Interference] The design interference was 0.03mm, but the low hot-shrinking temperature left only 0.015mm.
[Slipping] The torque required is T=μ·p·πdl·d/2, and since p∝δ, halving δ left insufficient torque, causing slipping and heating.
[Design Omission] The interference should be back-calculated from the starting torque with the hot-shrinking temperature controlled, but no torque verification was done.

Correct Solution

1) Raise the rotor interference to 0.03~0.04mm to guarantee torque transmission;
2) Control the hot-shrinking temperature at 230±10℃ to prevent annealing;
3) Calculate the required press force from T=μpπdl·d/2;
4) Specify shaft surface roughness Ra0.8 to improve bonding;
5) Dynamically balance to reduce vibration;
6) Monitor the assembly temperature by infrared measurement;
7) Verify torque transmission with a bench torque test;
8) Re-press out-of-specification rotors.

Checklist

References

GB/T 5371-2004 Interference Fit Calculation