Insufficient Hot-Assembly Temperature on the Yaw Bearing Ring Causes Loosening

E43-056 · Interference Fit Failures · Wind Turbine Yaw Bearing · ★★★

Problem Symptom

Designed interference between inner ring and shaft was 0.05mm but measured 0.02mm; the low hot-assembly temperature caused loosening, with abnormal noise and replacement

Root Cause

[Temperature Too Low] The design called for hot assembly at 220℃, but only 150℃ was used, giving insufficient expansion and an interference of just 0.02mm.
[Loosening] The expansion Δd=αdΔT depends on temperature rise; insufficient ΔT meant the mating surfaces were not clamped and the ring crept during operation.
[Design Omission] Sufficient temperature difference should be allowed for Δd=αdΔT and the actual interference measured, but the heating process was not controlled.

Correct Solution

1) Control the hot-assembly temperature at 220±10℃ to suit fitting over the bearing;
2) Calculate the thermal expansion from Δd=αdΔT to guard against over- or under-expansion;
3) Heat uniformly and hold the temperature so that the expansion is consistent;
4) Mark the final seated position to prevent incomplete seating;
5) Measure the torque after cooling to verify contact;
6) Locate the inner ring on its end face to prevent misalignment;
7) Re-tighten with a torque wrench to prevent loosening;
8) Reassemble out-of-specification parts.

Checklist

References

GB/T 307.3-2017 Rolling Bearings — General Technical Rules