Knowledge Base › Tolerance and Fit Error Case › Oversize Plating Substrate Causing Poor Coating Adhesion and Peeling

Oversize Plating Substrate Causing Poor Coating Adhesion and Peeling

E43-618 · Surface roughness mismatched with the fit · A chromium-plated shaft designed pre-plate Ra0.8 but measured Ra3.2, the coating bonds poorly and peels and spalls in service · ★★

Problem Description

The substrate before chrome plating at Ra3.2 is too rough; the coating bonds poorly to the base metal and peels and spalls under load.

Root Cause

[Mechanism] Plating adhesion depends on a clean, moderately rough substrate; on an oversize surface the coating stress concentrates at groove bottoms, bonding is poor, and spalling follows.
[Calculation] At Ra3.2 the coating thickness is uneven at groove bottoms, adhesion drops about 30% versus Ra0.8, and peeling occurs under shear.
[Design Omission] The pre-plate substrate roughness is wrong, a design defect → coating peeling.

Corrective Solution

1) Grind the substrate to Ra0.4~0.8 before plating;
2) Set substrate Ra per the plating process;
3) Activate and remove oxide before plating;
4) On the first article, verify substrate Ra and adhesion;
5) Specify pre-plate Ra on the drawing;
6) Grind to the finished Ra after plating;
7) Test adhesion by a cross-cut test;
8) Verify no spalling under a load test.

Checklist

Reference

GB/T 131-2006 Geometrical product specifications — Surface texture designation

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL