E43-633 · Surface Roughness Mismatch with Fit · A worm tooth surface designed Ra0.4 but measured Ra1.6, causing poor meshing oil film, heat, wear and low efficiency · ★★
The worm tooth surface is too rough at Ra1.6; the sliding-contact oil film breaks down, causing heat, wear and reduced drive efficiency.
[Mechanism] Worm drives have high sliding at the tooth mesh; excessive roughness breaks the oil film into boundary friction, generating heat and wear that lower efficiency.
[Calculation] With λ<1 mixed lubrication, a higher friction coefficient drops efficiency from 80% to 70%, and a 20℃ tooth-surface temperature rise accelerates wear.
[Design Omission] The worm tooth surface was left too rough; this design defect causes heating and wear.
1) Grind/polish the worm tooth surface to Ra0.2~0.4;
2) Set tooth-surface Ra by drive requirements;
3) Match a bronze worm gear to a hardened worm;
4) Measure tooth-surface Ra and temperature rise on the first article;
5) Mark the tooth Ra on the drawing;
6) Match lubricant viscosity;
7) Run in to break off peaks;
8) Test efficiency and temperature rise on a rig.
GB/T 131-2006 Geometrical product specifications — Surface texture designation