Cam Working Face Too Rough, Follower Wear and Impact

E43-634 · Surface Roughness Mismatch with Fit · A valvetrain cam face designed Ra0.4 but measured Ra1.6, causing early follower wear, inaccurate lift and motion impact · ★★

Problem Description

The cam working face is too rough at Ra1.6; the follower wears rapidly in contact, lift deviates, and motion produces impact and noise.

Root Cause

[Mechanism] The cam and follower are in high-pair contact; excessive roughness peaks raise contact stress and wear, and profile wear makes lift inaccurate, causing impact.
[Calculation] Stress-concentrating peaks raise the wear rate; after tens of thousands of cycles the profile wears 0.05, and lift deviation causes valvetrain impact.
[Design Omission] The cam face was left too rough; this design defect causes wear and impact.

Corrective Solution

1) Grind/polish the cam face to Ra0.2~0.4;
2) Surface-harden the cam to HRC55+;
3) Set Ra by contact requirements;
4) Measure Ra and profile on the first article;
5) Call out cam-face Ra on the drawing;
6) Match follower material;
7) Ensure adequate lubrication;
8) Test lift and wear in endurance.

Checklist

Reference

GB/T 131-2006 Geometrical product specifications — Surface texture designation

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL