E43-636 · Surface Roughness Mismatch with Fit · A hydrostatic guide face designed Ra0.4 but measured Ra1.6, causing pocket-land leakage and reduced oil-film stiffness · ★★
The hydrostatic guide face is too rough at Ra1.6; land leakage increases, and oil-film load capacity and stiffness drop, causing instability.
[Mechanism] A hydrostatic guide is load-carrying by its oil film; a too-rough sealing land increases leakage so pocket pressure cannot build, and load capacity and stiffness drop.
[Calculation] Land leakage scales with gap³ including a roughness equivalent; Ra1.6 raises leakage by about 50%, lowering oil-film stiffness and causing instability.
[Design Omission] The hydrostatic face was left too rough; this design defect causes oil-film leakage and reduced load capacity.
1) Grind/scrape the hydrostatic guide face to Ra0.4;
2) Match land width to Ra;
3) Match the restrictor to the pocket;
4) Measure Ra and oil-film pressure on the first article;
5) Call out hydrostatic-face Ra on the drawing;
6) Filter the oil to keep it clean;
7) Monitor oil-film thickness;
8) Test load capacity and stiffness.
GB/T 131-2006 Geometrical product specifications — Surface texture designation