E43-644 · Surface Roughness Mismatch with Fit · A journal designed Ra0.2 to retain oil but measured Ra0.02 (over-polished), causing poor oil retention and startup dry-friction wear · ★★
The journal was over-polished to Ra0.02; the surface has no oil-retaining micro-pits, and at startup there is momentary dry-friction wear.
[Mechanism] Moderately rough micro-pits store lubricating oil; over-polishing removes this oil-retention capacity, so at start/stop the oil film has not yet formed and dry contact occurs.
[Calculation] At Ra0.02 oil storage tends to zero; the first few startup turns have no oil film, peak contact raises the wear rate, and long-term journal wear results.
[Design Omission] Over-polishing lost oil retention; this design defect causes startup wear.
1) Hold the journal at Ra0.1~0.2 to keep oil-retaining micro-pits;
2) If needed, laser-texture oil-retaining pockets;
3) Set Ra by lubrication requirements;
4) Measure Ra and oil retention on the first article;
5) Call out the Ra lower limit on the drawing;
6) Pre-lubricate before startup;
7) Match oil grade;
8) Test wear in start/stop endurance.
GB/T 131-2006 Geometrical product specifications — Surface texture designation