E43-645 · Surface Roughness Mismatch with Fit · An oil-seal journal designed with nondirectional texture but found spiral turning marks causing a pumping effect and one-way seepage · ★★
Turning left a spiral texture on the journal; rotation creates a pumping effect and the oil seal leaks one-directionally.
[Mechanism] Residual spiral machining texture on the journal pumps oil directionally as it rotates; aligned with the pumping direction it drives oil out past the seal, causing seepage.
[Calculation] The spiral helix angle creates an axial pumping velocity; when aligned with the pumping direction it drives oil out of the seal, and seepage appears within hours.
[Design Omission] Texture direction was not controlled; this design defect causes pumping and seepage.
1) Superfinish/polish the seal journal to remove spiral marks;
2) Require nondirectional texture per GB/T;
3) Control texture helix angle ≈0;
4) Measure texture direction on the first article;
5) Call out nondirectional texture on the drawing;
6) Use transverse grinding instead of turning;
7) Use a double-lip seal against one-way leakage;
8) Run a rotating seepage test.
GB/T 131-2006 Geometrical product specifications — Surface texture designation