E43-649 · Surface Roughness Mismatch with Fit · A mold cavity mating surface designed for ground Ra0.8 but actually EDM at Ra3.2 with a recast layer, leading to early fatigue cracking · ★★
The EDM surface was left at Ra3.2 with a recast layer, so the fit fatigued and cracked early, with a short service life.
[Mechanism] EDM surfaces carry a recast layer, microcracks, and roughness; under alternating load these provide many crack initiation sites and cause early fatigue failure.
[Calculation] EDM at Ra3.2 with a recast layer cuts the fatigue strength by about 30%, so the fit surface cracks early under alternating load.
[Design Omission] The EDM surface received no post-treatment; design defect → early fatigue cracking.
1) Grind or polish after EDM to remove the recast layer down to Ra0.8;
2) Shot-peen to introduce compressive stress for fatigue resistance;
3) Set the surface Ra and treatment based on fatigue demand;
4) Inspect the first article for Ra and recast layer;
5) Mark the post-treatment on the drawing;
6) Use finish EDM settings to minimize the recast layer;
7) Crack inspection;
8) Verify by fatigue testing.
GB/T 131-2006 Geometrical product specifications — Surface texture designation