E43-703 · Taper and Angle Fit Error · Taper interference connection where the H/s taper-diameter band caused excessive interference, the press force exceeded equipment capacity, and the taper expansion split the hub · ★★★★
For a taper interference connection, the taper-diameter tolerance band was chosen wrongly (too much interference); the press force exceeded the press capacity, and after forcing it in, the taper expansion stress exceeded the limit and the hub’s taper bore split.
[Mechanism] Taper interference is controlled by the taper-diameter tolerance and the press-in amount; a wrong band makes the interference too large, the press stress exceeds the material strength, and the part splits.
[Calculation] An interference 0.1mm above design raises the taper contact pressure, pushes the hub inner-wall tangential stress past yield, and causes cracking.
[Design Omission] The taper interference tolerance band was miscalculated; the design defect leads to excessive interference and splitting.
1) Recalculate the taper interference tolerance band by elasticity theory;
2) Verify the press force and hub stress;
3) Control the press-in amount within tolerance;
4) On the first article, measure the press force and stress;
5) Achieve a taper contact rate ≥85%;
6) Verify the hub material strength;
7) Specify the taper-diameter tolerance on the drawing;
8) Verify by press fitting.
GB/T 1800.1-2020 Geometrical product specifications (GPS) - Limits and fits