Stainless-Steel Thread Seizing and Galling

E43-738 · Thread Tolerance and Fit Error · A 304 stainless bolt and nut seized during engagement, would not turn, and forcing it tore the threads and ruined both · ★★★

Problem Description

A 304 stainless-steel bolt and nut seized (cold-welded) during engagement: the threads suddenly locked solid and would not turn, and forcing them tore the flanks, ruining both bolt and nut.

Root Cause

[Mechanism] Stainless steel conducts heat poorly and its oxide film breaks easily; the friction heat of engagement makes the flanks locally cold-weld, seize, and tear.
[Calculation] Stainless steel has a high friction coefficient; heating at the engaging contact points breaks the oxide film and cold-welds the flanks, the seizure torque spikes, and the threads tear.
[Design Omission] The stainless threads were given no anti-seize treatment - a design defect leading to seizing and tearing.

Corrective Solution

1) Molybdenum-disulfide / anti-seize the stainless threads;
2) Control assembly speed to avoid overheating;
3) Refine thread Ra to reduce asperity contact;
4) On first articles, confirm engagement seizes not;
5) Stagger bolt and nut material hardness;
6) Avoid high-speed engagement under load;
7) Call out anti-seize requirements on the drawing;
8) Verify mating.

Checklist

Reference

GB/T 197-2018 General-purpose metric screw threads — Tolerances