E43-744 · Thread Tolerance and Fit Error · A thread-rolled bolt's pitch diameter crept up as the dies wore, pushing a later batch over the upper limit and letting oversize parts slip through sampling · ★★★
During thread-rolling bolt production, the rolling dies wore gradually; the bolt pitch diameter crept from acceptable to oversize, and a later batch ran past the 6g upper limit. Sampling gaps missed it, letting out-of-tolerance parts through that were too interference to enter the nut.
[Mechanism] Worn rolling dies make the rolled pitch diameter grow over time; without process monitoring, a later batch goes out of tolerance and sampling misses it.
[Calculation] Die wear raises the pitch diameter 0.02mm per 10,000 parts; later continuous production passes the upper limit, and out-of-tolerance parts slip in between sampling intervals.
[Design Omission] There was no continuous monitoring of pitch diameter during rolling - a design defect leading to batch out-of-tolerance and missed rejection.
1) Sample-check the pitch diameter at set intervals during rolling;
2) Monitor die wear and replace in time;
3) Use SPC to monitor the pitch-diameter trend;
4) Inspect GO/NO-GO with a ring gauge;
5) Measure pitch diameter on first and in-process parts;
6) Keep rolling parameters stable;
7) Specify sampling frequency in the process sheet;
8) 100% inspect suspect batches.
GB/T 197-2018 General-purpose metric screw threads — Tolerances