E43-750 · Thread Tolerance and Fit Error · A same-material, same-hardness bolt and nut gall on engagement, with torque spiking and seizure during tightening · ★★★
When bolt and nut are of the same material and hardness (similar HRC), the engaging flanks gall and seize: the torque spikes during tightening, the joint locks locally, and forcing it further tears the thread flanks.
[Mechanism] Thread pairs of the same hardness gall on contact; the hardness should be staggered into a soft-on-hard combination to reduce adhesion. Otherwise the flanks gall and seize.
[Calculation] Same-hardness flanks have a high tendency to adhere; under assembly friction they cold-weld, the torque spikes, and the joint seizes and tears.
[Design Omission] The bolt and nut hardnesses were not staggered — a design defect leading to galling and seizure.
1) Stagger bolt and nut hardness (difference ≥HRC 5);
2) Apply surface treatment (phosphate / plating) to prevent galling;
3) Apply lubricant;
4) On first articles, measure the assembly torque;
5) Refine the thread surface roughness Ra;
6) Control the assembly speed;
7) State the hardness pairing on the drawing;
8) Verify mating.
GB/T 197-2018 General-purpose metric screw threads — Tolerances