E43-749 · Thread Tolerance and Fit Error · A titanium bolt-and-nut assembly scuffs and galls, causing abnormal assembly torque and thread seizing on disassembly · ★★★
During assembly, the titanium-alloy bolt and nut scuff and gall at the contacting surfaces: the assembly torque fluctuates abnormally, and on disassembly the thread flanks weld and scuff, making them hard to remove and damaging the threads.
[Mechanism] Titanium alloys are highly reactive and prone to adhesion; under the friction of thread engagement the flanks gall and scuff, the torque goes abnormal, and the joint seizes on disassembly.
[Calculation] Titanium has a high friction coefficient and tends to adhere; the engaging flanks micro-weld and scuff 0.02mm deep, raising the disassembly torque and seizing the joint.
[Design Omission] The titanium threads were given no anti-galling surface treatment — a design defect leading to scuffing and seizing.
1) Treat titanium threads (anodize / coat) to prevent galling;
2) Apply a dedicated anti-seize lubricant;
3) Control the assembly speed;
4) On first articles, test assembly and disassembly;
5) Refine the thread surface roughness Ra;
6) Avoid matching the bolt and nut materials;
7) State the anti-galling treatment on the drawing;
8) Assemble/disassemble verification.
GB/T 197-2018 General-purpose metric screw threads — Tolerances