Excessive Hot-Assembly Temperature Anneals the Bearing Inner Ring

E43-263 · Rolling Bearing Fit Errors · Vertical Motor Bearing Inner Ring ∅70, hot assembly specified at 80~100℃ but actual 160℃ · ★★

Problem Symptom

Hot assembly at 160℃ (allowable 120) annealed the ring and dropped the hardness from HRC60 to 52, cutting the contact fatigue life by 50%

Root Cause

[Mechanism] The excessive temperature tempered the ring and reduced its hardness.
[Calculation] The tempering temperature exceeded 120℃, decomposing the martensite and dropping the hardness from HRC60 to 52, so the contact fatigue life L∝(HRC)^k fell by about 50%.
[Design Omission] The heating temperature was not controlled; this design flaw caused the annealing failure.

Correct Solution

1) Control the heating to 80~100℃ to prevent tempering;
2) Use temperature-controlled induction heating to prevent overheating;
3) Measure the hardness HRC≥60 to verify the material;
4) Use a spacer to avoid direct heating of the ring;
5) Inspect the clearance after installation;
6) Run in and listen for abnormal noise;
7) Spot-check the hardness;
8) Bring the process temperature into the specification.

Checklist

References

JB/T 8881 Rolling Bearings — Heat Treatment of Parts