Knowledge Base › Tolerance and Fit Error Case › Spiral-Wound Gasket Compression Out of Tolerance - Insufficient Recovery

Spiral-Wound Gasket Compression Out of Tolerance - Insufficient Recovery

E43-891 · Seal and Clearance Fit Error · A heat-exchanger spiral-wound gasket designed compression 25% measured 45% (flange spacing too small), over-compressing the gasket, yielding the windings and defeating the seal · ★★★

Problem Description

A spiral-wound gasket in a shell-and-tube heat exchanger was compressed to 45% instead of the designed 25% because the flange-face spacing was too small; the V-shaped metal windings are over-flattened and yield, the recovery rate drops sharply, and after thermal cycling the gasket loses compensation and leaks.

Root Cause

[Mechanism] A spiral-wound gasket creates contact pressure by elastic compression of the V-shaped windings and recovers to compensate; excessive compression makes the windings plastically yield and lose elastic recovery reserve.
[Calculation] Compression ε = compression / free thickness, recommended 15%~30%; the measured 45% exceeds the yield threshold, and the unloaded recovery drops from about 15% to below 5%, leaving no compensation.
[Design Omission] The flange-face spacing (stop) was machined too small without controlling the maximum compression — a design defect leading to over-compression, yielding, insufficient recovery and seal failure.

Corrective Solution

1) Add a flange stop ring to hold compression at 25%±5% and prevent over-compression;
2) Size the stop height from ε = compression / free thickness, quantitatively;
3) Inspect incoming spiral-wound gasket free thickness and recovery rate;
4) Back-calculate bolt torque from the compression and protect with a stop;
5) Tighten symmetrically in stages while monitoring compression, holding the upper limit;
6) On first articles, unload and measure recovery ≥12%, to verify;
7) Call out compression and stop-ring dimensions on the drawing;
8) Replace over-compressed gaskets and add a stop ring.

Checklist

Reference

GB/T 4622.2-2008 Spiral-wound gaskets — Dimensions