E43-920 · Seal and Clearance Fit Error · A high-temperature valve O-ring compression set designed ≤20% measured 45% (material heat resistance insufficient), so recovery fails after long compression, contact pressure goes to zero and it leaks · ★★★
A high-temperature steam valve O-ring used nitrile material with insufficient heat resistance, giving a compression set measured at 45%, above the designed ≤20%; after long high-temperature compression the O-ring stays permanently flattened, loses recovery, and contact pressure goes to zero and leaks.
[Mechanism] An O-ring maintains sealing contact pressure by elastic recovery after compression; excessive compression set means it cannot recover on unloading, and contact pressure accumulates to zero and loses the seal.
[Calculation] Residual compression = initial compression − permanent set; a 45% set > the about 25% initial compression leaves negative residual compression, contact pressure goes to zero, and it leaks.
[Design Omission] The material heat-resistance class was insufficient and material was not selected for temperature — a design defect leading to high set, lost recovery and leak.
1) Select material by working temperature (FKM / silicone) and hold set ≤20%;
2) Measure compression set per GB/T 7759, quantitatively;
3) Inspect incoming material heat-resistance class;
4) Hold compression within the recommended range to cut set;
5) For high-temperature service, prefer metal/graphite seals;
6) On first articles, measure recovery after high-temperature aging, to verify;
7) Call out material grade, heat resistance and set on the drawing;
8) If material fails, replace with a heat-resistant grade.
GB/T 7759.1-2015 Vulcanized rubber — Determination of compression set