E43-335 · Thermal Deformation Uncompensated · A fixture disc-spring stack preloaded to 5000N, designed 60℃ rise, measured preload drop · ★★
A 60℃ temperature rise relaxed the disc springs and dropped preload 8%, causing insufficient clamping and workpiece shift.
[Mechanism] Heating lowers the disc-spring elastic modulus and causes creep; preload decays with temperature rise and clamping is insufficient.
[Calculation] Modulus drops about 8%/100℃; at ΔT=60℃ preload drops about 8% = 400N, leaving clamping insufficient.
[Design Omission] No hot-state preload check or pressure make-up — a design defect leading to insufficient clamping.
1) Make up pressure to 5400N for the 8% hot preload drop;
2) Insulate the disc springs to hold rise ≤30℃;
3) Monitor clamp force in real time and alarm;
4) Select high-temperature disc-spring material to hold modulus;
5) Periodically re-measure preload;
6) Add a mechanical lock to prevent loosening;
7) On first articles, measure clamp force;
8) Monitor workpiece shift during machining.
GB/T 1972-2005 Disc springs