E43-343 · Thermal Deformation Not Compensated · A nozzle 300mm long, designed positioning, measured rise 40℃ with elongation · ★★
A 40℃ nozzle temperature rise elongates it by 0.138mm, misaligning the nozzle from the gate and causing flash.
[Mechanism] The nozzle expands axially under heat, misaligning it from the mold gate; the seal fails and flash results.
[Calculation] α=11.5e-6, Δl=11.5e-6×300×40=0.138mm, exceeding the 0.1mm alignment tolerance and causing flash.
[Design Omission] No compensation for nozzle thermal elongation in alignment — a design defect leading to flash.
1) Pre-adjust nozzle alignment for the 0.138mm hot elongation;
2) Add cooling to the nozzle to hold the rise ≤20℃;
3) Add a locating bushing at the mold gate to prevent misalignment;
4) Monitor nozzle temperature in real time;
5) Use low-expansion nozzle material to reduce Δl;
6) Add elastic compensation at the sealing face;
7) Inspect the first article for flash;
8) Re-check alignment periodically.
JB/T 7267-2004 Plastics injection molding machines