Weld Distortion Shifts Hole Positions

E43-049 · Weld/Cast Forming Out of Tolerance · Welded Frame · ★★

Problem Symptom

Hole positions shifted 1.2mm after welding; the reaming allowance was insufficient; 20% rework rate

Root Cause

[Weld Distortion] Transverse shrinkage of the fillet weld shifted the hole positions by 1.2mm, because weld shrinkage had not been pre-allowed for.
[Shift] The displaced holes left less than 0.3 of reaming allowance, so they could not be corrected.
[Design Omission] Weld shrinkage should be pre-allowed, the holes bored after welding or process bosses provided, and the welding sequence was not controlled.

Correct Solution

1) Reserve weld shrinkage allowance to prevent dimensional contraction;
2) Bore the holes after welding to guarantee positional accuracy;
3) Provide process bosses for auxiliary location to prevent distortion;
4) Optimise the welding sequence and use symmetric welding to reduce warping;
5) Stress-relief anneal after welding to remove distortion;
6) Measure hole positions on a CMM on the first piece to verify position;
7) Control weld distortion using the back-step method;
8) Bring weld distortion control into the process specification.

Checklist

References

GB/T 19804-2005 Welded Structures — Dimensional Tolerances