Casting Shrinkage Causes a Pit at the Mating Surface

E43-050 · Weld/Cast Forming Out of Tolerance · Cast Iron Housing · ★★

Problem Symptom

Casting shrinkage produced a Φ8×2 deep pit at the bearing bore; 10 parts scrapped per month

Root Cause

[Shrinkage] Insufficient feeding at the wall thickness transition formed a Φ8 shrinkage cavity 2 deep, which was exposed after machining.
[Pit] Local lack of material at the bearing seat bore left the support surface unsupported and deformed the bearing outer ring.
[Design Omission] Risers should be provided for feeding, the wall thickness should be uniform, NDT performed after rough machining, and the casting process was not controlled.

Correct Solution

1) Provide risers for feeding to eliminate shrinkage and ensure soundness;
2) Make wall thickness transitions uniform to prevent stress cracking;
3) Use magnetic particle or ultrasonic inspection after rough machining to find defects;
4) Add reinforcing bosses at the bearing bore to raise rigidity;
5) Carry out a casting process qualification to guarantee stability;
6) Section the first piece to verify internal quality;
7) Leave adequate machining allowance to avoid cutting into shrinkage cavities and scrapping parts;
8) Bring casting quality into incoming inspection.

Checklist

References

GB/T 9439-2010 Grey Iron Castings