E43-373 · Welded/Cast Forming Dimensional Error · A rotary turntable 1500mm diameter, designed radial runout 0.05, measured post-weld 0.22 · ★★
Welding distortion of the turntable pushes radial runout 0.22mm out of tolerance, causing rotational eccentricity.
[Mechanism] Release of residual stress from fabricated welding warps the turntable face, offsetting the rotation center.
[Calculation] Radial runout≈2e=2×0.11=0.22mm (e eccentricity), 4.4× the tolerance of 0.05.
[Design Omission] No post-weld finish turning or aging — a design defect leading to runout error.
1) Overall age after welding to relieve stress;
2) Finish-turn the turntable face to hold runout;
3) Provide a process datum hole;
4) Weld symmetrically in segments;
5) Control heat input;
6) Measure runout with a dial indicator;
7) Align the center;
8) First-article runout measured ≤0.05mm.
GB/T 1184-1996 Shape and position tolerances - Undefined tolerances