Pressure-Vessel Head Spinning Thinning Error

E43-379 · Welded/Cast Forming Dimensional Error · A head 1200mm diameter, 10mm plate, designed thinning ≤1, measured 2.8 · ★★

Problem Description

Spinning/stretching the head thins the crown by 2.8mm, leaving insufficient strength.

Root Cause

[Mechanism] During head spinning the plate is stretched and thinned; the crown thins most and exceeds tolerance.
[Calculation] Thinning rate≈(10-7.2)/10=28%; the 2.8mm thinning is 2.8× the tolerance of 1.
[Design Omission] No control of the spinning process or thickened blank — a design defect leading to wall-thickness error.

Corrective Solution

1) Oversize the head blank by 2.8mm to compensate;
2) Optimize the spinning stretch ratio;
3) Control even blank-holder force;
4) Form in multiple passes to reduce thinning;
5) 100% inspect with a thickness gauge;
6) Improve die surface finish;
7) Design a thickened crown zone;
8) Measure first-article wall thickness to spec.

Checklist

Reference

GB/T 25198-2010 Pressure vessel heads