Welded Oil-Tank Wall-Plate Distortion Causing Flatness Error

E43-386 · Welded/Cast Forming Dimensional Error · A tank wall plate 1500×1000mm, designed flatness 1.0, measured post-weld 4 · ★★

Problem Description

Weld shrinkage warps the tank wall plate, pushing flatness 4mm out of tolerance and bulging the skin.

Root Cause

[Mechanism] Uneven weld shrinkage warps the thin plate; the wall bulges off the plane.
[Calculation] Flatness w≈σ·L²/(8Eh)=20×1500²/(8×110000×4)≈0.13 (4mm measured), 4× the tolerance of 1.
[Design Omission] No internal support or segmented welding — a design defect leading to flatness error.

Corrective Solution

1) Use an internal support fixture during welding to hold the shape;
2) Weld thin plate in segmented skip passes with low heat input;
3) Flatten after welding;
4) Add temporary stiffeners;
5) Control the welding sequence;
6) Stress-relieve after welding;
7) Check flatness with a straight edge;
8) Measure first-article flatness ≤1.0mm.

Checklist

Reference

GB/T 1804-2000 General tolerances — Tolerances for linear and angular dimensions without individual tolerance indications