Knowledge Base › Tolerance and Fit Error Case › Large Ingot-Mold Distortion Causing Cast-Billet Size Error

Large Ingot-Mold Distortion Causing Cast-Billet Size Error

E43-387 · Welded/Cast Forming Dimensional Error · An ingot-mold cavity 400×400, designed side 400±1, measured distorted 406 · ★★

Problem Description

Thermal distortion of the ingot mold expands the cavity by 6mm, pushing the cast billet out of tolerance.

Root Cause

[Mechanism] The ingot mold repeatedly expands and distorts under heat; cavity dimensions grow, pushing the cast billet out of tolerance.
[Calculation] Cavity growth Δ≈α·ΔT·L=11.5e-6×200×400≈0.92 (6mm measured with creep), 6× the tolerance of 1.
[Design Omission] No mold-temperature control or deformation allowance — a design defect leading to cavity error.

Corrective Solution

1) Control mold working temperature ≤200℃;
2) Reinforce the mold wall against expansion;
3) Measure cavity dimensions periodically;
4) Provide even-temperature cooling;
5) Use heat-resistant mold material;
6) Replace out-of-tolerance molds;
7) Check the cavity with a template gauge;
8) Measure first-article billet ≤1mm.

Checklist

Reference

GB/T 8491-2009 Heat-resistant cast iron castings

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »