Casting Aging Distortion Driving Datum Hole Spacing Out of Tolerance

E43-400 · Welding and Casting Dimensional Error · A housing with a 400mm datum hole spacing designed at 400±0.05 that measured 400.28 after aging · ★★

Problem Description

Long-term stress relief of the casting displaced the datum holes by 0.28mm, mislocating the parts.

Root Cause

[Mechanism] Slow relaxation of residual stress inside the casting shifts the hole pattern slightly, putting the spacing out of tolerance.
[Calculation] The spacing change Δ≈σ·L/E=22×400/110000≈0.08 (compounding with the measured 0.28), 5.6 times the 0.05mm tolerance.
[Design Omission] Inadequate artificial aging — a design defect leading to hole-spacing error.

Corrective Solution

1) Thermally stress-relieve before rough machining;
2) Add a second aging step between rough and finish machining;
3) Use symmetric wall thickness;
4) Measure the hole-spacing datum before machining;
5) Low-stress fixturing;
6) Measure hole spacing on a CMM;
7) Provide process pads;
8) Measure first-article hole spacing ≤0.05mm.

Checklist

Reference

GB/T 9439-2010 Grey cast iron castings