E44-311 · Excessive Pipe Resistance and Pressure Drop · Unground internal weld seams at Ra=12.5μm · ★★
Actual λ=0.035 exceeds the 0.022 design value, raising hf by 60%; the friction loss of 0.3MPa exceeds the 0.18 allowance.
[Roughness] The weld bead raises the equivalent roughness ε and drives λ up.
[Rising Resistance] λ moving from 0.022 to 0.035 raises hf (∝λ) by 60%.
[Design Omission] No control of inner-wall roughness and no grinding of weld seams — roughness out of spec.
1) Grind internal weld seams to Ra≤3.2μm, since the original 12.5 gave λ=0.035 (over 0.022) and +60% hf — thus cutting roughness and λ;
2) Check λ from the design ε with the Colebrook equation, since larger ε raises λ and hf — thus sizing λ correctly;
3) Choose smooth-bore pipe (e.g., PE-lined), since roughness adds loss — thus smoothing the wall;
4) On long lines, prioritize low roughness to save power, since hf accumulates with L — thus weighting roughness;
5) Clean the line on schedule to preserve the wall, since scale adds roughness — thus keeping it smooth;
6) Check hf=λL/d·v²/2g with the actual λ, since an assumed λ starves the end — thus using the true value;
7) Boost pump head to cover the added resistance, since the end needs pressure, adding head;
8) Fold inner-wall roughness into quality control, since the unchecked roughness was the root cause — thus locking it in at QC.
GB/T 20801.3-2020 Design code for industrial metallic piping