E44-965 · Vessel Strength and Wall-Thickness Deficiency · Pressure vessel · ★★★
Fatigue cracking, leakage, fracture
[Mechanism] The vessel sees alternating pressure; the stress range at nozzles and supports exceeds the fatigue limit, and cycles accumulate until cracks grow and leak.
[Calculation] Δp=1.0MPa, stress range Δσ=110MPa, material fatigue limit 90MPa, cracking after 2×10⁵ cycles.
[Design Omission] No fatigue-life check, no stress-range reduction, and no periodic inspection.
1) Check fatigue life N=2×10⁶ cycles (was under 2×10⁵), since Δσ over the limit caused cracking and the life check shows the margin — thus preventing cracking;
2) Lower the stress range (smooth transition R≥50mm brings Δσ down to 80MPa), since a large range cracks and cutting it extends life — thus suppressing cracking;
3) Replace sharp corners with smooth transitions, since corners concentrate stress and transitions ease it — thus suppressing concentration;
4) Perform periodic NDE (MT every 5000 cycles), since cracks appear early and can be repaired — thus monitoring cracking;
5) Run fatigue testing (verify N≥2×10⁶), since the life was never checked and measurement confirms it — thus setting fatigue life by data;
6) Fit a cycle counter (alarm on over-limit), since fatigue shows as cycles before cracking — thus monitoring cycles and warning early;
7) In operation, hold Δp≤0.8MPa (reduce if exceeded), since a large range cracks and range control prevents it — thus running to prevent cracking;
8) Write the life check and range reduction into the calculation book, since the cracking root cause was Δσ over the limit unchecked — thus locking it in at design.
GB/T 150.1-2011 Pressure vessels