Welding Defect Leak

E44-966 · Vessel Strength and Wall-Thickness Deficiency · Weld seam · ★★★

Problem Description

Welding defect, leakage, cracking

Root Cause

[Mechanism] The weld was not NDE-inspected; lack-of-fusion and porosity defects grew under pressure and corrosion into a leak.
[Calculation] The weld was not inspected; defects rated Class IV (out of spec), and at 1.6MPa the defect-site σ=210MPa grew into a leak.
[Design Omission] No NDE, no welding-procedure qualification, and insufficient welder qualification.

Corrective Solution

1) Perform RT/UT inspection (Class I acceptance, repair out-of-spec), since weld defects are the leak source and finding them lets you repair — thus removing defects;
2) Qualify the welding procedure (WPS compliant), since a wrong procedure causes defects and a qualified process is reliable — thus assuring process quality;
3) Use certified welders (process-matched), since poor welding causes defects and certified welders make strong seams — thus assuring weld quality;
4) Run a hydrotest (1.25× design pressure held 30min for leak detection), since micro-leaks first show as seepage and measurement confirms — thus setting sealing by data;
5) Run an air-tightness test (soapsuds check at 0.05MPa), since micro-leaks are hard to see and gas makes them visible — thus detecting micro-leaks;
6) Post-weld heat treatment to relieve stress (600℃ annealing), since residual stress causes cracking and heat treatment removes it — thus relieving stress;
7) Control weld quality (inspect each pass), since poor work causes defects and quality control makes strong seams — thus controlling welding;
8) Write the NDE procedure into the process card, since the leak root cause was missed inspection and a wrong procedure — thus locking it in by process.

Checklist

Reference

GB/T 150.1-2011 Pressure vessels