E44-994 · Vessel Strength and Wall-Thickness Deficiency · Shell · ★★★
Out-of-round, stress, deformation
[Mechanism] The formed shell was out of round; under internal pressure the hoop stress is unevenly distributed, locally exceeding allowable and prone to fatigue.
[Calculation] Out-of-roundness e=15mm (limit e≤1%D=18mm, but on the high side), local stress rises 18%, local σ=210MPa exceeds [σ].
[Design Omission] No roundness check, no rolling/calibration, and no roundness inspection.
1) Check roundness (e≤0.5%D=9mm to control stress), since large e raises stress and calibration lowers it — thus lowering stress;
2) Re-roll the shell (calibrating roll to e≤9mm), since eccentricity stresses and rolling evens it — thus rounding;
3) Add internal bracing to prevent distortion (hold round during fit-up), since a soft shell goes eccentric and bracing keeps it round — thus preserving roundness;
4) Raise the wall to 10mm (was 8mm), since a thin wall goes eccentric and a thick one raises stiffness — thus reinforcing;
5) Measure roundness (one point every 2m, e≤9mm), since eccentricity first shows in the roundness and can be calibrated early — thus monitoring roundness;
6) Run a hydrotest (1.25× design pressure), since out-of-roundness causes stress and measurement confirms stability — thus setting strength by data;
7) Control assembly quality (hold to roundness inspection points), since poor assembly goes eccentric and controlled assembly evens it — thus compliant assembly;
8) Write the roundness check and rolling into the process card, since the high-out-of-roundness root cause was the missed check and no rolling — thus locking it in by process.
GB/T 150.1-2011 Pressure vessels