E44-1008 · Vessel Strength and Wall-Thickness Deficiency · Pressure vessel · ★★★
Dense openings, weak, cracking
[Mechanism] Multiple openings were closely spaced; reinforcement zones overlapped and the overall weakening exceeded GB/T 150 allowance.
[Calculation] 4×DN80 in a 300mm zone, single opening needs 1200mm², overlap double-counted, total need 18000mm², supplied only 9000mm², local σ=205MPa exceeds.
[Design Omission] No opening-spacing control, no combined reinforcement calc, and no stress check.
1) Control opening spacing (≥2d, staggered), since close spacing weakens and even layout distributes it — thus distributing the weakening;
2) Run a combined reinforcement calc (A total need ≥18000mm², supply enough), since under-reinforcement concentrates stress and a correct calc provides enough — thus lowering stress;
3) Add an integral reinforcing ring (covering the cluster), since a weak zone cracks and a ring reinforces it — thus reinforcing;
4) Switch to a thicker shell (δ=12mm, was 8mm), since a thin wall is weak and a thick one raises strength — thus raising strength;
5) Perform MT on the opening cluster (no cracks), since cracks first show as lines and can be rejected early — thus finding cracks;
6) Run a hydrotest (1.25× design pressure), since under-reinforcement caused cracking and measurement confirms stability — thus setting strength by data;
7) Control adjacent spacing (≥2.5d, non-overlapping reinforcement zones), since overlap weakens and controlled spacing distributes — thus laying out openings;
8) Write the spacing control and reinforcement calc into the calculation book, since the dense-openings root cause was the missed combined A calc and small spacing — thus locking it in at design.
GB/T 150.1-2011 Pressure vessels