E44-1007 · Vessel Strength and Wall-Thickness Deficiency · Pressure vessel · ★★★
Negative tolerance unaccounted, thin wall, leak
[Mechanism] The steel's rolling negative tolerance (-12.5%) was not included in the design wall, so the actual wall fell below the calculated need.
[Calculation] Nominal δ=8mm, -12.5% actual 7.0mm, need 7.6mm, short by 0.6mm, σ 8% over.
[Design Omission] No negative-tolerance accounting, no actual-wall check, and no allowance.
1) Add negative tolerance C1=0.25δ to the design (nominal 8mm takes 2mm → specify nominal 10mm), since actual 7.0<needed 7.6 caused a shortfall and the added allowance makes it up — thus restoring thickness;
2) Check actual wall (re-measure on delivery ≥ nominal - tolerance), since negative tolerance thins and the check reveals it — thus monitoring thickness;
3) Add corrosion allowance C2 (by corrosion rate), since corrosion stacks on negative tolerance and an allowance leaves margin — thus resisting corrosion;
4) Switch to thicker material (nominal 10mm, actual ≥8.75mm), since a thin wall is short and a thick one raises strength — thus reinforcing;
5) Ultrasonic thickness-test (every point ≥7.6mm), since negative tolerance first shows as a thin wall and can be replaced early — thus monitoring thickness;
6) Run a hydrotest (1.25× design pressure), since the thin-wall leak was untested and measurement confirms no seepage — thus setting strength by data;
7) Hold service stress ≤90% of design (margin kept), since exceeding it risks a thin wall and stress control stabilizes — thus running to prevent thinning;
8) Write the tolerance accounting and wall check into the calculation book, since the unaccounted-tolerance root cause was the missed C1 and unchecked actual wall — thus locking it in at design.
GB/T 150.1-2011 Pressure vessels