E44-047 · Other · Flue-Gas Duct Bellows Expansion Joint · ★★
Fatigue cracked the bellows over 80mm and caused leakage; failure occurred after 8000h of service.
[Fatigue] Cyclic displacement drives the bellows stress amplitude beyond the fatigue limit; life N=(Δε)^-2.
[Rupture] Too few convolutions make each convolution absorb too much displacement.
[Design Omission] Fatigue life was not checked and displacement was not controlled; rupture caused leakage.
1) Size the convolution count by fatigue life; cyclic displacement pushes the bellows stress amplitude past the fatigue limit, life N=(Δε)^-2, cracking at 8000h, so set convolution count by life;
2) Keep per-convolution displacement within the design limit; large per-convolution displacement overshoots the stress amplitude, so limit the displacement;
3) Add guide supports to limit displacement; guides constrain displacement and cut per-convolution overload, so add guidance;
4) Install the expansion joint with preset deformation; preset deformation distributes displacement and extends life, so pre-deform;
5) Periodically inspect appearance and wall thickness; cracks start where the wall thins, so inspect;
6) Provide leak collection and alarm; leakage is hazardous, so alarm it;
7) Verify displacement compensation on commissioning; compensation is proven by testing, so verify it;
8) Bring fatigue assessment into expansion-joint selection; the original failure to check life was the root cause of cracking, so selection must include it.
GB/T 12777-2017 Metal bellows expansion joints