E44-1085 · Other · Rupture Disk · ★★
Premature rupture, burst, discharge.
[Mechanism] The disk was rated for 1.0MPa burst, but Cl⁻ in the medium corroded it down to an actual 0.7MPa; the normal operating peak of 0.8MPa then triggered a premature rupture, defeating protection and discharging the medium.
[Calculation] Design burst p_b=1.0MPa; after corrosion actual p_b'=0.7MPa; operating peak p_op=0.8MPa>p_b', so premature; margin (p_op-p_b')/p_b'=14%, which fails to meet ≥1.1× operating pressure (should be ≥0.88MPa), and the disk bursts at peak pressure.
[Design Omission] No corrosion-environment burst check, no corrosion-resistant material, no burst test, and no pressure-monitoring alarm.
1) Choose a corrosion-resistant rupture disk (Hastelloy replacing 304); Cl⁻ corrosion cut burst resistance to 0.7, and changing material restores 1.0, recovering the rated burst pressure;
2) Check burst pressure ≥1.1× operating pressure (take 1.1MPa>0.8 peak); low pressure causes premature rupture, and a checked pressure leaves margin, preventing it;
3) Add a corrosion barrier layer (coating / isolation film); corrosion cuts resistance, and isolation protects, extending disk life;
4) Control cyclic fatigue (limit start-stops to design cycles); fatigue weakens, and limiting frequency stabilizes, preventing gradual cracking;
5) Run a burst test (sampled burst within ±5%); missing tests leave parameters unknown, and measured pressure confirms it;
6) Install pressure monitoring (alarm above 0.8); premature rupture first shows as a pressure rise, and early warning catches it;
7) Set a replacement interval (by corrosion rate, ≤2 years); long corrosion weakens, and controlled intervals replace it, preventing in-service mis-rupture;
8) Record burst-pressure check and corrosion-resistant selection on the rupture-disk drawing; the root cause of premature rupture was no corrosion-pressure check and non-resistant material, so the drawing must gate it.
GB/T 567-2012 Rupture disc safety devices