E44-1099 · Other · Conveying Pipe · ★★
Blocked, conveying, stopped.
[Mechanism] Powder moisture was too high and caked; air velocity was below suspension velocity; material piled at the line bottom and blocked it.
[Calculation] Material moisture 3% (should be ≤1%); suspension velocity u_t=12m/s; conveying air velocity v=9m/s<u_t; blockage rate 5 times per shift.
[Design Omission] No moisture control, no air-velocity check, no blow-out, and no conveyance test.
1) Control air velocity ≥15m/s (>u_t=12); low velocity blocks, and adequate velocity suspends material, preventing settling;
2) Control moisture ≤1% (dry the 3% feed); high moisture sticks, and low moisture disperses, preventing caking;
3) Check bore matched to air volume (hold velocity); a large bore drops velocity, and a checked bore holds speed, conveying freely;
4) Add a blow-out valve (auto-blow at blockage points); deposition blocks, and blowing clears it, restoring conveyance;
5) Run a conveyance test (8h continuous without blockage); untested means unknown, and measured flow confirms it;
6) Install material-flow monitoring (alarm on flow loss); a blockage first shows as flow loss, and early warning catches it;
7) Set a cleaning interval (every shift); long intervals block, and controlled intervals keep it clean, preventing blockage;
8) Record air velocity and moisture control on the conveying drawing; the root cause of blockage was low air velocity and high moisture, so the drawing must gate it.
GB/T 50050-2017 Industrial circulating cooling water